トレランス モンテカルロ
What is the yield of this stack under production variation?
数千サンプルにわたる層ごとの膜厚および Refractive index 変動をシミュレートし、実際の製造トレランス下でのスタック設計の挙動を確認できます。
How it works
Manufacturing tolerance analysis samples the stack's forward model many times with layer thickness and index perturbed by their process standard deviations. The resulting distribution of the specified metric (band-averaged reflectance, colour shift, et cetera) gives the percentile bands and the yield at a given acceptance limit. The sensitivity of the yield to each parameter follows from the partial derivatives of the metric at the nominal design.
Worked example
Kriya 4-layer broadband, ±3 nm / ±0.01 n, 500 runs
Monte Carlo over thickness + n tolerances; σ(R) and yield-at-spec.
Validation method, references and test-case results: /validation#tolerance-mc