How do I extract refractive index and thickness from a transmission spectrum?

コーティング膜の透過スペクトルと裸基板のリファレンスから、Refractive index n(λ)、Extinction coefficient k(λ)、および物理膜厚 d を抽出します。多孔質シリカ LRI コーティング向けに自社開発した Low refractive index(n < s)ブランチの閉形式解法も含みます。

How it works

The Swanepoel envelope method fits two smooth curves to the maxima and minima of a transmission spectrum through a thin film on a transparent substrate. The ratio and separation of the envelopes give the refractive index and the thickness; the absorption coefficient follows from the envelope average. The result depends only on the spectrum and the substrate index.

Worked example

a-Si:H envelope from Swanepoel 1983 Table 1

Transmission envelope → thickness, n(λ) via Swanepoel 1983.

Validation method, references and test-case results: /validation#swanepoel