Stoney応力 & 基板反り

What curvature does a stressed film induce in its substrate?

測定された基板曲率から等二軸薄膜応力を計算、または目標応力に対するウェハー反りを予測。12種類の基板材料。

How it works

Stoney's equation relates the biaxial stress in a thin film to the curvature it induces in a much thicker substrate, given the substrate's biaxial modulus and thickness and the film thickness. The equation assumes an elastic substrate, a uniform film stress and a film-to-substrate thickness ratio below a few percent. Measured curvature therefore gives a direct read-out of residual stress for thin coatings.

Worked example

Si(100), E 130 GPa, ν 0.28, 525 µm substrate, 1 µm film, R 10 m

Inputs: substrate = silicon_100, substrateThicknessUm = 525, filmThicknessNm = 1.000e+3, radiusOfCurvatureM = 10

Result: 829.4 MPa

Reference: Stoney 1909 Proc. R. Soc. A 82, 172; Freund & Suresh 2003 §2.3

Computed by this tool's kernel at build (commit dae6663).

Validation method, references and test-case results: /validation#stoney-stress

Request accessOpen the interactive tool