NIR太陽熱取得シミュレーター(ATO)
How much solar heat gain does an ATO-loaded window block?
ガラス構成とATOナノ粒子充填量を与えると、SHGC、VLT、車室内温度の予測低減量、AC消費電力の低減、BEVの場合は航続距離影響を計算します。
How it works
Solar heat gain through glazing is set by the integral of the solar spectrum against the glazing's transmittance, weighted by the fraction absorbed and re-radiated inward. Antimony tin oxide nanoparticles absorb selectively in the near infrared while transmitting most of the visible band, so loading an interlayer with ATO reduces solar heat gain more than visible light transmittance. Downstream cabin temperature and compressor-energy effects follow from standard automotive thermal models.
Worked example
Beer–Lambert: α 1.0 mm⁻¹, path 3 mm
Inputs: alphaPerMm = 1, pathMm = 3
Result: 4.979 %
Reference: Hecht §4.4; standard Beer–Lambert exp(−αd)
Computed by this tool's kernel at build (commit dae6663).
Validation method, references and test-case results: /validation#solar-heat-ato