LRI 粒子設計モデル
How does nanoparticle loading change the refractive index of a coating?
第一原理から低屈折率コーティングを設計:中空ナノ粒子の形状(殻厚、直径、充填密度)が二段階有効媒質理論を介して有効屈折率を決定します。
How it works
Adding nanoparticles to a polymer host shifts the effective refractive index of the mixture toward the index of the particles. Effective-medium theories (Maxwell-Garnett at low fractions, Bruggeman at higher) relate the loading, host and particle indices to the mixture index. Process-side constraints on viscosity and film continuity bound the practical loading range.
Worked example
Hollow silica 60 nm, shell 8 nm, 55 vol % in binder 1.49
Hollow-silica particles in a binder; Maxwell-Garnett for both the particle and film mixing steps.
Validation method, references and test-case results: /validation#lri-particle