LIDARウィンドウ透過率計算機

How much signal does the cover window lose for a 905 nm or 1550 nm LiDAR?

905、940、または1550 nmにおいて、LIDARカバーウィンドウへのKriya AR添加による往復透過率向上を計算します。

How it works

A LiDAR cover window sees the emission pulse twice — once outbound, once on the return. Each pass is attenuated by the coated window's transmittance at the laser wavelength, so the signal returned to the detector scales as the square of the single-pass transmittance. A narrow-band anti-reflection coating recovers most of the loss at the design wavelength.

Worked example

Lossless incoherent slab, n 1.52: R_total = 2R / (1 + R)

Inputs: nSlab = 1.52

Result: 8.168 %

Reference: Born & Wolf §1.6.3 — thick-slab incoherent sum

Computed by this tool's kernel at build (commit dae6663).