有効媒質計算機
What refractive index does a nanoparticle-in-matrix mixture have?
複合・多孔質・ナノ粒子コーティングの有効屈折率:順方向または逆方向、vol % または wt %、出典明記の材料カタログ付き。
How it works
Effective-medium theories model a composite of small inclusions in a host matrix as a homogeneous medium with an averaged dielectric function. Maxwell-Garnett is valid at low filler fractions with isolated inclusions; Bruggeman handles higher loadings where inclusions percolate. The predicted effective index depends on the inclusion volume fraction, the host and inclusion dielectric functions, and the characteristic inclusion size relative to the wavelength.
Worked example
Maxwell–Garnett: air in SiO₂ (n 1.46), f 0.30
Inputs: nHost = 1.46, nInclusion = 1, volumeFraction = 0.3
Result: 1.321
Reference: Maxwell Garnett 1904; Aspnes 1982 Thin Solid Films 89, 249
Computed by this tool's kernel at build (commit dae6663).
Validation method, references and test-case results: /validation#effective-medium