色シフト/レインボー指数
How much does the reflected colour change with viewing angle?
CIE測色を用いて、人間の観察者から見た多層スタックの角度依存色シフト(「レインボー」)を定量化します。
How it works
Reflected spectra from thin films depend on the optical path length through each layer, which lengthens with increasing angle of incidence. Integrating the angle-dependent reflectance against a reference illuminant gives the reflected colour; the perceptual shift between two angles is quantified by the CIE ΔE* colour-difference metric in a uniform colour space such as CIELAB.
Worked example
CIEDE2000 Sharma pair 1
Inputs: lab1 = {"L":50,"a":2.6772,"b":-79.7751}, lab2 = {"L":50,"a":0,"b":-82.7485}
Result: 2.042 ΔE₀₀
Reference: Sharma, Wu & Dalal 2005 Color Res. Appl. 30, 21
Computed by this tool's kernel at build (commit dae6663).
Validation method, references and test-case results: /validation#colour-shift