課題

The display OEM needed a reliable single-source supplier for antistatic colour-filter coating for their global PDP production. The volume requirement was 120+ metric tonnes in the first year alone, scaling to sustained production over multiple years.

02

アプローチ

Kriya scaled production from zero to 120 MT within the first year (2009), becoming the sole global supplier of antistatic colour-filter coating for PDP. Manufacturing quality was ensured through ISO 9001 processes with every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.

03

成果

Over four years (2010–2014), Kriya supplied approximately 500,000 kg as the sole global supplier. Zero supply disruptions. The engagement validated Kriya’s manufacturing capability and quality systems at production scale.

Kriyaの強み

Kriya demonstrated the ability to scale from lab to 100+ MT production in under a year, with the quality systems and supply reliability demanded by a global display OEM.