全ケーススタディ
ディスプレイ — 折りたたみ

PFASフリーフレキシブルARがWCA >100°を達成、PFASより優れた保持力

韓国の大手ディスプレイTier-1メーカー

主要指標

>100°水接触角(PFASフリー)
SuperiorPFAS比WCA保持率
Pass防汚耐久性
R2R量産対応

01

課題

With PFAS regulation tightening globally, the display OEM needed a PFAS-free anti-reflective and anti-fouling solution for foldable displays that could match or exceed the surface property retention of incumbent PFAS-based coatings under repeated mechanical stress.

02

アプローチ

Kriya’s PFAS-free ARAF technology, based on functionalised HSiO₂ nanoparticles, was tested against PFAS-based references for water contact angle, anti-smudge durability, and retention after steel wool abrasion cycles. The formulation was designed for UV cure compatibility with R2R processing.

03

成果

The PFAS-free coating achieved WCA above 100° with superior retention versus PFAS-based alternatives after repeated abrasion. Anti-smudge properties (fingerprint resistance and marker wipe-off) were maintained across the full test protocol. The coating is R2R-compatible for volume production.

Kriyaの強み

Kriya provides a complete PFAS-free alternative that actually outperforms PFAS on durability retention, eliminating regulatory risk while improving product performance.

主要指標

>100°水接触角(PFASフリー)
SuperiorPFAS比WCA保持率
Pass防汚耐久性
R2R量産対応

使用製品

関連アプリケーション

Displays — Foldable →

同様のアプリケーションについて相談

当社の技術チームが、お客様の要件に対する適用可能性を評価します。

お問い合わせ