全ケーススタディ
自動車サーマル

太陽熱制御ガラスによりEV航続距離16 km延長

EVモデル車両を対象に調査を実施

主要指標

+16 km航続距離延長(プレミアムセグメント)
€325車両あたりバッテリー節約
35%エアコン消費電力削減
100%5G/RF/LiDAR透過

01

課題

The EV manufacturer needed to extend vehicle range without increasing battery size, which adds weight and cost. AC power consumption in warm climates was identified as a significant parasitic load, particularly during the regulatory shift toward stricter EU CO₂ targets that penalise each g/km above target at €95 per vehicle.

02

アプローチ

Kriya’s ATO solar heat control glazing was modelled for the premium EV segment (85.6 kWh average battery, 442 km WLTP range). The integration blocks 250 W/m² of NIR solar radiation while remaining fully transparent to 5G, RF, and LiDAR signals—a critical requirement that ITO-based alternatives cannot meet.

03

成果

The analysis showed up to 16 km range extension, 8.5 kg battery saving equivalent to approximately €325 per vehicle, and 35% AC power reduction. For the compact segment (39.3 kWh, 227 km), the extension was 7 km with 4.6 kg battery saving worth approximately €159.

Kriyaの強み

Unlike ITO alternatives, Kriya ATO does not block RF signals, making it the only viable solar heat control solution for connected and autonomous vehicles.

主要指標

+16 km航続距離延長(プレミアムセグメント)
€325車両あたりバッテリー節約
35%エアコン消費電力削減
100%5G/RF/LiDAR透過

使用製品

関連アプリケーション

Automotive Thermal →

同様のアプリケーションについて相談

当社の技術チームが、お客様の要件に対する適用可能性を評価します。