全ケーススタディ
ディスプレイ

多層ARスタックで広帯域反射率0.15%以下を達成

大手Tier-1ディスプレイ光学フィルムメーカー

主要指標

<0.15%残留反射率
+3.3%透過率向上(PET)
100%全基材での密着性
4検証済み基材数

01

課題

The consumer-electronics company required a broadband anti-reflective coating stack achieving residual reflectance below 0.15% across the visible spectrum. The solution had to be PFAS-free and compatible with their existing substrate portfolio (PET, PC, PMMA, TAC).

02

アプローチ

Kriya designed a multi-layer AR stack utilising the full RI platform from 1.16 to 1.95. The stack was optimised through optical modelling and validated on four substrates, measuring transmission gain, haze, reflection, pencil hardness, and adhesion per ISO and ASTM standards.

03

成果

Broadband residual reflectance below 0.15% was achieved on the multi-layer stack. Transmission gains ranged from 2.2% (PMMA) to 3.3% (PET), with 100% adhesion on all substrates. Pencil hardness varied by substrate from HB (PC) to 4H (PMMA). All formulations were PFAS-free.

Kriyaの強み

Kriya offers the widest PFAS-free RI range (1.16–2.00) from a single supplier, enabling complete multi-layer AR stacks without sourcing from multiple vendors.

主要指標

<0.15%残留反射率
+3.3%透過率向上(PET)
100%全基材での密着性
4検証済み基材数

使用製品

関連アプリケーション

Displays →

同様のアプリケーションについて相談

当社の技術チームが、お客様の要件に対する適用可能性を評価します。

お問い合わせ