全ケーススタディ
自動車サーマル

ATO分散液がPVB中ヘイズ0.2〜0.3%を達成、Tier-1中間膜パートナーが検証

Tier-1 PVB中間膜メーカー

主要指標

<0.3%ヘイズ(自動車グレード)
5×同等SHGC時の競合比効果
~60%ITO比コスト
75%可視光透過率

01

課題

The Tier-1 PVB interlayer partner needed an ATO dispersion for solar heat control interlayer film that could achieve automotive-grade haze (<0.5%) when laminated with green glass. Previous ATO suppliers using top-down ball-milling produced dispersions with haze exceeding 1.7%, far above automotive requirements.

02

アプローチ

Kriya provided four ATO dispersion variants at 8.3 wt% concentration for evaluation. The partner laminated samples with 2.0 mm green glass and measured optical properties including visible light transmission, total solar transmittance, and haze according to their internal automotive qualification protocol.

03

成果

The optimised variant achieved 0.2% haze at 0.10 wt% and 0.3% haze at 0.20 wt% in PVB—the only samples passing the partner’s automotive haze threshold. Visible light transmission ranged from 71–75%, and total solar transmittance from 58–61%. The partner concluded the technology had "great potential."

Kriyaの強み

Kriya’s proprietary bottom-up ATO synthesis produces nanoparticles with fundamentally lower scattering than ball-milled alternatives, achieving 5× better effectiveness at equal SHGC versus the leading competitor.

主要指標

<0.3%ヘイズ(自動車グレード)
5×同等SHGC時の競合比効果
~60%ITO比コスト
75%可視光透過率

使用製品

関連アプリケーション

Automotive Thermal →

同様のアプリケーションについて相談

当社の技術チームが、お客様の要件に対する適用可能性を評価します。

お問い合わせ