照明

Edge-lit glass light panel

Luminous glass for buildings, furniture and signage

A glass pane lit from its edge glows wherever an extraction pattern sends the light out. As soon as the pane is laminated, bonded or held by a material of similar index, the light escapes there instead. A low-index coating on the glass keeps the light guided — and lets the panel be laminated into safety glass or bonded into a frame.

FRONTBACKCover glass (optional)Laminated or bondedInterlayer or adhesivePVB, EVA or OCA · n ≈ 1.48 · not KriyaLow-index coatingKeeps the light in the guideLight-guide glass with edge LEDsLow-iron glass · n 1.52Extraction patternPrint, etch or laserReflector or back glass (optional)Not KriyaK1
公開済み Kriya ポジション適合 Kriya ポジションその他の層
全層リスト (6)
  1. Cover glass (optional) Laminated or bonded
  2. Interlayer or adhesive PVB, EVA or OCA · n ≈ 1.48 · not Kriya
  3. Low-index coating Keeps the light in the guideK1
  4. Light-guide glass with edge LEDs Low-iron glass · n 1.52
  5. Extraction pattern Print, etch or laser
  6. Reflector or back glass (optional) Not Kriya

参考文献

  1. US 6,742,921 — Light pipe, plate light source unit and reflection type liquid-crystal display device — 2000 priority: a layer bonded to a light guide through a lower-index layer, so that guided light is totally reflected at the interface
  2. EP 1 447 433 — Coating material composition and article having coating film formed therewith — 2001 filing: low-index coating from fine hollow particles in a binder

模式図であり、縮尺は正確ではありません。