自動車

Automotive LiDAR

The sensor cover in the laser path

A LiDAR fires near-infrared pulses — usually at 905 nm or 1550 nm — through a cover, often an infrared-transparent, visibly black polycarbonate, and catches the echo through the same cover. Each bare PC surface reflects about 5 %, and the light crosses the cover twice: on the way out and on the way back.

OUTSIDESENSORAR topcoat — low indexn ≈ 1.30 · UV-curable · thickness set for 905or 1550 nmAR basecoat — high indexn ≈ 1.75 · UV-curable · ≈ 3 µmPolycarbonate coverIR-transparent, visibly black · n ≈ 1.58AR on the inner faceSensor-cavity sideAir (sensor cavity)LiDAR emitter and receiver905 nm or 1550 nmK1K1K2
公開済み Kriya ポジション適合 Kriya ポジションその他の層
全層リスト (5)
  1. AR topcoat — low index n ≈ 1.30 · UV-curable · thickness set for 905 or 1550 nmK1
  2. AR basecoat — high index n ≈ 1.75 · UV-curable · ≈ 3 µmK1
  3. Polycarbonate cover IR-transparent, visibly black · n ≈ 1.58
  4. AR on the inner face Sensor-cavity sideK2
  5. LiDAR emitter and receiver 905 nm or 1550 nm

参考文献

  1. US 6,210,858 — Anti-reflection film and display device using the same — 1997 filing: wet-coated anti-reflection film with hard coat, high-index layer and a low-index layer (n 1.20–1.55) that owes its index to micro voids
  2. H. A. Macleod, Thin-Film Optical Filters, 3rd edition (2001), chapter 3: Antireflection coatings — multi-layer designs for the visible; sections 3.4 and 3.5: coatings with two zeros, and coatings for the visible and the infrared together · link: publisher page of the current edition

関連する Kriya ページ

このページで使用する Kriya ツール

模式図であり、縮尺は正確ではありません。