AR glasses — holographic waveguide
A holographic waveguide couples light in and out with volume gratings recorded in a photopolymer or liquid-crystal layer only a few micrometres thick. The substrates around it can be thin glass or plastic of ordinary index, so the range of guided angles is narrow from the start. Every layer added outside the guide — a cover, a second colour plate, a laminate — has to be separated from it by something of very low index.
全層リスト (9)
- Hard coat, AR and easy-clean On the world-side coverK1
- World-side cover Bonded with optical adhesive · not Kriya
- Low-index layer 0.5–2 µm · n ≈ 1.2K2
- Substrate Glass or polymer, 50–500 µm · n ≈ 1.52
- Holographic grating layer Photopolymer or liquid-crystal polymer, 2–5 µm · not Kriya
- Substrate Glass or polymer
- Low-index layer 0.5–2 µm · n ≈ 1.2K2
- Eye-side cover plate Bonded with optical adhesive · not Kriya
- Hard coat and multi-layer AR Eye sideK1
作業方法
バージョン 1 · 公開日A low-index layer on both outer faces of the guide, flat covers bonded over it, coated outer faces.
このコーティングの塗布方法 — 工程、公的な基盤、そしてデバイスメーカーに残される要素。
- Coat both outer faces of the guide with a low-index layer
n about 1.2, 0.5–2 µm. Against n 1.20 an n 1.52 guide guides beyond 52.1°. For polymer substrates: n 1.21 with an 80 °C cure, UV-curable from n 1.30.
対象層: Low-index layer - Bond flat covers over it
Optical adhesive on the low-index layer. Adhesive and covers are not Kriya.
対象層: World-side cover · Eye-side cover plate - Coat the outer faces
Hard coat (3H+ to 4H), multi-layer AR (R < 0.15 %) and an easy-clean top layer with a water contact angle above 100° without fluorinated chemistry.
対象層: Hard coat, AR and easy-clean · Hard coat and multi-layer AR
公開済みの根拠
技術水準を示す、選定された期限切れ特許、論文、書籍、規格。
- US 6,742,921 — Light pipe, plate light source unit and reflection type liquid-crystal display device — 2000: a layer bonded to a light guide through a lower-index layer; guided light is totally reflected at that interface.
- EP 1 447 433 — Coating material composition and article having coating film formed therewith — 2001: a low-index coating made of fine hollow particles in a binder.
デバイスメーカーに残る部分
The grating layer, its recording and the layout of the guide.
本記述は法的助言ではありません。
参考文献
- B. Kress, Optical waveguide combiners for AR headsets: features and limitations — Proc. SPIE 11062, 110620J (2019)
- US 6,742,921 — Light pipe, plate light source unit and reflection type liquid-crystal display device — 2000 priority: a layer bonded to a light guide through a lower-index layer, so that guided light is totally reflected at the interface
- EP 1 447 433 — Coating material composition and article having coating film formed therewith — 2001 filing: low-index coating from fine hollow particles in a binder
模式図であり、縮尺は正確ではありません。