Épaisseur humide d'applicateur

How thick must the wet coat be to leave this dry film thickness?

Prédit l'épaisseur de film humide à partir des réglages d'applicateur : Mayer bar, slot-die, héliogravure ou enduction par centrifugation.

How it works

The dry film thickness of a coating equals the wet film thickness multiplied by the volume solids fraction of the formulation. The volume solids fraction follows from the solvent mass fraction, the formulation density and the solvent density. Coating-method process windows set the practical range of wet thickness.

Worked example

Slot-die on 1 m web at 10 m/min, 50 ml/min metered flow → 5 µm wet

Mass-balance wet thickness for Mayer bar, slot-die, gravure or spin.

Validation method, references and test-case results: /validation#wet-thickness

Request accessOpen the interactive tool