Calculateur de tension de bande
What web tension suits this coated substrate?
Définit une tension de bande sûre pour films polymères minces et feuille d'aluminium à partir de la résistance à la traction du substrat, de la section et d'un facteur de sécurité choisi.
How it works
A coated web must be transported at a tension high enough to avoid wrinkling and low enough to avoid substrate stretch or coating damage. The window is set by the substrate's modulus, the coating's elastic limit and the line geometry. A simple force balance gives the recommended tension for each process station.
Worked example
PET 50 µm × 1 m wide at 60 m/min
Minimum and target web tension from substrate yield and curvature radius.
Validation method, references and test-case results: /validation#web-tension