Simulateur de réflectance en couches minces TMM

How do I design or analyse a thin-film optical stack?

Calcule la réflectance et la transmittance d'un empilement optique multicouche arbitraire à l'aide de la méthode de la matrice caractéristique (matrice de transfert).

How it works

The transfer-matrix method describes propagation of light through a stack of parallel homogeneous layers by multiplying a two-by-two characteristic matrix per layer. Each matrix captures the layer's phase thickness and admittance, derived from its refractive index and physical thickness. Combining the per-layer matrices gives the stack's amplitude reflection and transmission coefficients at any wavelength and angle.

Worked example

BK7 Sellmeier at 550 nm

Inputs: wavelength = 550

Result: 1.519

Reference: Schott BK7 datasheet (DL-5-82) via Macleod 5th ed. app. 3

Computed by this tool's kernel at build (commit dae6663).

Validation method, references and test-case results: /validation#tmm

Request accessOpen the interactive tool