Calculateur de retrait au durcissement

How much does this resin shrink on cure?

Estime l'épaisseur de film sec, la perte volumétrique et le facteur d'augmentation de densité dus au retrait au durcissement de la famille chimique choisie.

How it works

A curing resin shrinks as its monomers polymerise into a denser network. The shrinkage fraction depends on the monomer chemistry and the achieved degree of cure. The induced residual stress adds to any thermal-mismatch stress in the finished coating.

Worked example

UV acrylate, 5 % volume shrinkage, 10 µm wet film

Constrained-film cure shrinkage: all volume loss projected into thickness.

Validation method, references and test-case results: /validation#cure-shrinkage

Request accessOpen the interactive tool