Flat optics & imaging

Metalens

A flat lens made of sub-wavelength pillars

A metalens replaces a curved lens with millions of nanopillars whose width sets the local phase delay. To cover a full 2π of phase at a practical height, the pillars need a high index against their surroundings. Imprinting them directly in a high-index nanocomposite replaces deposition and etching for every part; a low-index embedding layer makes them robust.

LIGHT INLIGHT OUTLow-index embedding layerProtects the pillars; can carry an AR or bebondedNanopillarsImprinted high-index nanocompositeResidual layerSame resin as the pillarsSubstrateGlass wafer · n ≈ 1.46–1.52Backside anti-reflectionLow-index or multi-layer ARK1K2K2K3
Kriya coating position — published on kriya-materials.comKriya chemistry applies — application fit from public literatureOther device layers — not supplied by Kriya
All layers (5)
  1. Low-index embedding layer Protects the pillars; can carry an AR or be bondedK1
  2. Nanopillars Imprinted high-index nanocompositeK2
  3. Residual layer Same resin as the pillarsK2
  4. Substrate Glass wafer · n ≈ 1.46–1.52
  5. Backside anti-reflection Low-index or multi-layer ARK3

Schematic, not to scale. Layer order, indices and thicknesses are typical values from the public references; real devices differ by maker and generation. Kriya values as published on kriya-materials.com. Kriya formulates every coating for the customer's substrate, process and specification.