Energy, buildings & agriculture

Greenhouse glazing

More light for the crop through the same glass

At higher latitudes, natural light limits crop growth in greenhouses through autumn and winter. Each bare glass surface reflects 4.3 % at normal incidence — about 8 % for the two faces of a pane — before the light reaches the crop. Anti-reflection on both faces recovers most of that, and an anti-soiling top coat helps keep the roof clean.

SUNCROPAnti-soiling top coatOuter faceAnti-reflection, outer facePorous low-index layerGreenhouse glassClear or diffuse, ≈ 4 mm · n 1.52Anti-reflection, inner facePorous low-index layerK2K1K1
Kriya coating position — published on kriya-materials.comKriya chemistry applies — application fit from public literatureOther device layers — not supplied by Kriya
All layers (4)
  1. Anti-soiling top coat Outer faceK2
  2. Anti-reflection, outer face Porous low-index layerK1
  3. Greenhouse glass Clear or diffuse, ≈ 4 mm · n 1.52
  4. Anti-reflection, inner face Porous low-index layerK1

Public references

  1. F. Kempkes et al., Increase of light transmission by 10% in the Venlo-type greenhouse: from design to results of a cucumber experiment — Acta Horticulturae 1296 (2020): diffuse glass with an anti-reflective coating among the measures; light transmission increased by more than 10 %
  2. New glass coatings for high insulating greenhouses without light losses — energy saving, crop production and economic potentials — Acta Horticulturae 893 (ISHS): anti-reflection coatings on greenhouse glass

More on kriya-materials.com

Kriya tools used on this page

Schematic, not to scale. Layer order, indices and thicknesses are typical values from the public references; real devices differ by maker and generation. Kriya values as published on kriya-materials.com. Kriya formulates every coating for the customer's substrate, process and specification.