Eye tracking lights the eye with near-infrared emitters, typically around 850 or 940 nm, and films it with a small camera. The tracker looks for the reflections of the emitters on the cornea, which reflects only 2.5 %. In headsets, and in glasses worn with prescription inserts, a lens sits between tracker and eye, and each of its surfaces mirrors the emitters back into the camera. A lens coated for visible light only can be worse than no coating at all.
All layers (7)
- Visible + near-infrared AR Eye-side surface of the lensK1
- Hard coat Carries the AR stackK3
- Lens between tracker and eye Prescription insert or headset lens · n 1.5–1.67
- Hard coatK3
- Visible + near-infrared AR Tracker-side surface of the lensK1
- Near-infrared AR on the camera windowK2
- Eye tracker: emitters and camera Outside the lens, looking through it · 850 or 940 nm · not Kriya
Working method
Version 1 · first publishedOne AR stack for the visible and the tracker's band on both surfaces of the lens; emitters and camera stay outside the lens.
Step by step: where each layer goes, its index, its thickness and how it is cured. Compositions are not part of it. Point at a step to see its layers.
- Hard coat on both sides of the lens
Pencil hardness 3H+ to 4H; index matched to the lens, up to 1.65.
Layers: Hard coat - AR for the visible and the tracker's band
Thin-film model on n 1.52: four layers alternating n 1.30 and n 1.95, 155 / 23 / 61 / 21 nm from the air side. On average 0.8 % over the visible, 0.3 % at 850 nm, 0.55 % at 940 nm, and the lens stays transparent further into the infrared. A visible-only stack reflects about 10 % at 940 nm.
Layers: Visible + near-infrared AR - Quarter-wave low-index layer on the camera window
n 1.30, about 180 nm for 940 nm: 0.3 % instead of 4.3 % per surface (thin-film model).
Layers: Near-infrared AR on the camera window
Public basis
Earlier public documents that describe the same steps.
- US 4,145,122 — Method and apparatus for monitoring the position of the eye — 1979: infrared emitter and detector carried by a spectacle frame.
- H. A. Macleod, Thin-Film Optical Filters, 3rd edition (2001), chapter 3: Antireflection coatings — Textbook treatment of anti-reflection coatings with two zeros and of coatings that serve the visible and the infrared together.
- US 6,210,858 — Anti-reflection film and display device using the same — 1997: wet-coated AR built from a hard coat, a high-index layer and a low-index layer.
Stays with the device maker
Emitters and their optics, the camera, where they sit and the tracking software. This stack has no emitters and no infrared combiner inside the lens.
A working method describes how a coating can be applied. It is not legal advice. The design of a complete device, and clearing it against the rights of others, stays with the device maker.
Public references
- US 4,145,122 — Method and apparatus for monitoring the position of the eye — 1979 patent: infrared emitter and detector carried by a spectacle frame
- US 6,210,858 — Anti-reflection film and display device using the same — 1997 filing: wet-coated anti-reflection film with hard coat, high-index layer and a low-index layer (n 1.20–1.55) that owes its index to micro voids
- H. A. Macleod, Thin-Film Optical Filters, 3rd edition (2001), chapter 3: Antireflection coatings — multi-layer designs for the visible; sections 3.4 and 3.5: coatings with two zeros, and coatings for the visible and the infrared together · link: publisher page of the current edition
More on kriya-materials.com
Kriya tools used on this page
Schematic, not to scale. Layer order, indices and thicknesses are typical values from the public references; real devices differ by maker and generation. Kriya values as published on kriya-materials.com. Kriya formulates every coating for the customer's substrate, process and specification.