Smart glasses — laser scanning with a hologram in the lens
In laser-scanning glasses a small projector in the temple sweeps red, green and blue laser beams across the lens. A hologram inside the lens — a film a few tens of micrometres thick — diffracts the beams into the pupil while the rest of the lens looks like an ordinary prescription lens. The hologram does not survive heat, and the lasers hit the eye-side surface at a steep angle. Both facts decide which coatings can be used.
All layers (5)
- Hard coat, AR and easy-clean World sideK1
- Lens body, world side Lens polymer
- Hologram film inside the lens Embedded by the lens maker · photopolymer, stable to 60–120 °C · not Kriya
- Lens body, eye side Carries the prescription surface
- Hard coat and angle-tuned AR Eye side: first surface the laser meetsK1 · K2
Working method
Version 1 · first publishedEverything is applied to the finished lens and cured by UV light, below the hologram's temperature limit.
Step by step: where each layer goes, its index, its thickness and how it is cured. Compositions are not part of it. Point at a step to see its layers.
- UV-cured hard coat on both faces
Cured by UV light, so the lens stays below the hologram's limit of 60–120 °C. Pencil hardness 3H+ to 4H.
Layers: Hard coat, AR and easy-clean · Hard coat and angle-tuned AR - Low-index layer tuned to the laser's angle, eye side
n 1.30, about 134 nm for 520 nm at 60°: s-polarised reflection falls from 21 % to 2.8 %; with n 1.20, to 0.02 % (thin-film model).
Layers: Hard coat and angle-tuned AR - AR and easy-clean on the world side
Multi-layer AR, R < 0.15 %; water contact angle above 100° without fluorinated chemistry.
Layers: Hard coat, AR and easy-clean
Public basis
Earlier public documents that describe the same steps.
- US 5,246,728 — Scratch-resistant coating and method of making coated lenses — 1993: spin-coated hard coat on plastic lenses, cured by ultraviolet light.
- US 6,210,858 — Anti-reflection film and display device using the same — 1997: wet-coated AR built from a hard coat, a high-index layer and a low-index layer.
Stays with the device maker
The hologram, the way it is embedded in the lens, and the projector.
A working method describes how a coating can be applied. It is not legal advice. The design of a complete device, and clearing it against the rights of others, stays with the device maker.
Public references
- US 8,432,624 — Optical article and method for producing the same — fringes from index mismatch and thickness variation on n 1.67 and 1.74 lenses; oven cure at 125 °C
- US 5,246,728 — Scratch-resistant coating and method of making coated lenses — 1993 patent: spin-coated hard coat on plastic ophthalmic lenses, cured by ultraviolet light
- US 6,210,858 — Anti-reflection film and display device using the same — 1997 filing: wet-coated anti-reflection film with hard coat, high-index layer and a low-index layer (n 1.20–1.55) that owes its index to micro voids
More on kriya-materials.com
Kriya tools used on this page
Schematic, not to scale. Layer order, indices and thicknesses are typical values from the public references; real devices differ by maker and generation. Kriya values as published on kriya-materials.com. Kriya formulates every coating for the customer's substrate, process and specification.