AR & VR

AR glasses — freeform prism

One moulded prism folds the image; a second lens restores the view

A freeform prism folds the image inside a single moulded wedge. The light enters through one surface, is totally reflected at the eye-side surface, reflected again at the half-mirrored outer surface and then leaves through the same eye-side surface it was just reflected from. A second lens cemented to the outside restores the undistorted view of the world. The eye-side surface therefore has two jobs — mirror for steep rays, window for the rest — and it is the surface the wearer can touch.

WORLD SIDEDISPLAYHard coat and AR, world sideOn the auxiliary lensAuxiliary (compensator) lensCorrects the see-through viewOptical cementNot KriyaHalf-mirror on the prism's outersurfaceNot KriyaFree-form prismPMMA (n 1.49) or cyclo-olefin (n 1.53)Coating on the eye-side surfaceReflects by total internal reflection andtransmitsAirAR on the display-side entry surfaceMicro-displayNot KriyaK1K2K3
Kriya coating position — published on kriya-materials.comKriya chemistry applies — application fit from public literatureOther device layers — not supplied by Kriya
All layers (8)
  1. Hard coat and AR, world side On the auxiliary lensK1
  2. Auxiliary (compensator) lens Corrects the see-through view
  3. Optical cement Not Kriya
  4. Half-mirror on the prism's outer surface Not Kriya
  5. Free-form prism PMMA (n 1.49) or cyclo-olefin (n 1.53)
  6. Coating on the eye-side surface Reflects by total internal reflection and transmitsK2
  7. AR on the display-side entry surfaceK3
  8. Micro-display Not Kriya

Working method

Version 1 · first published

Hard coat and AR on the auxiliary lens, AR on the entry surface, an easy-clean layer on the surface that reflects by total internal reflection.

Step by step: where each layer goes, its index, its thickness and how it is cured. Compositions are not part of it. Point at a step to see its layers.

  1. Hard coat and AR on the auxiliary lens

    Hard coat 3H+ to 4H with multi-layer AR, R < 0.15 %, on the world side.

    Layers: Hard coat and AR, world side
  2. AR on the entry surface

    Single low-index layer, n 1.30, about 106 nm: about 0.5 % luminous reflectance on PMMA instead of 3.9 % (thin-film model).

    Layers: AR on the display-side entry surface
  3. Easy-clean layer on the eye-side surface

    A transparent coating leaves total internal reflection where it is, from 42.2°; a fingerprint (n ≈ 1.47) would move that limit to 80.6°. Water contact angle above 100° without fluorinated chemistry.

    Layers: Coating on the eye-side surface

Public basis

Earlier public documents that describe the same steps.

Stays with the device maker

Prism shape, half-mirror and display.

A working method describes how a coating can be applied. It is not legal advice. The design of a complete device, and clearing it against the rights of others, stays with the device maker.

Public references

  1. US 5,701,202 — Head or face mounted image display apparatus — 1995 filing: three-surface prism whose eye-side surface both totally reflects and transmits; see-through element cemented on
  2. US 6,210,858 — Anti-reflection film and display device using the same — 1997 filing: wet-coated anti-reflection film with hard coat, high-index layer and a low-index layer (n 1.20–1.55) that owes its index to micro voids

Schematic, not to scale. Layer order, indices and thicknesses are typical values from the public references; real devices differ by maker and generation. Kriya values as published on kriya-materials.com. Kriya formulates every coating for the customer's substrate, process and specification.