In a birdbath module the image from a micro-OLED display is folded by a flat beamsplitter and a curved, partially reflective mirror in front of the eye. The optics are simple and the image is sharp, but the light meets a half-mirror three times, and every surface that carries no mirror adds a faint copy of the image next to the real one. Those second surfaces are where anti-reflection coatings earn their place.

WORLD SIDEDISPLAYHard coat and easy-cleanOuter face of the shieldFront shieldTinted polycarbonateAR, inner face of the shieldAR on the mirror's convex sideWorld-facing second surfaceCurved half-mirror50–70 % reflective on the concave side ·mirror coating not KriyaAirAR on the beamsplitter's secondsurfaceEye-facing sideBeamsplitter40–60 % reflective · not KriyaAR on the display cover and relaylensMicro-OLED displayAbove the beamsplitter · not KriyaK1K2K2K2K3
Kriya coating position — published on kriya-materials.comKriya chemistry applies — application fit from public literatureOther device layers — not supplied by Kriya
All layers (9)
  1. Hard coat and easy-clean Outer face of the shieldK1
  2. Front shield Tinted polycarbonate
  3. AR, inner face of the shieldK2
  4. AR on the mirror's convex side World-facing second surfaceK2
  5. Curved half-mirror 50–70 % reflective on the concave side · mirror coating not Kriya
  6. AR on the beamsplitter's second surface Eye-facing sideK2
  7. Beamsplitter 40–60 % reflective · not Kriya
  8. AR on the display cover and relay lensK3
  9. Micro-OLED display Above the beamsplitter · not Kriya

Working method

Version 1 · first published

Anti-reflection on every surface that carries no mirror, a hard coat on the shield.

Step by step: where each layer goes, its index, its thickness and how it is cured. Compositions are not part of it. Point at a step to see its layers.

  1. AR on the uncoated second surfaces

    Convex side of the curved mirror and eye-facing side of the beamsplitter. Behind a 50 % mirror the ghost falls from 1.9 % of the image (bare PMMA) to 0.08 % with R < 0.15 %.

    Layers: AR on the mirror's convex side · AR on the beamsplitter's second surface
  2. Shield: AR inside, hard coat and easy-clean outside

    Hard coat 3H+ to 4H on polycarbonate; easy-clean with a water contact angle above 100° without fluorinated chemistry.

    Layers: AR, inner face of the shield · Hard coat and easy-clean
  3. AR on the display cover and relay lens

    Multi-layer AR, R < 0.15 %.

    Layers: AR on the display cover and relay lens

Public basis

Earlier public documents that describe the same steps.

Stays with the device maker

Mirror and beamsplitter coatings, polarization films and the optical layout.

A working method describes how a coating can be applied. It is not legal advice. The design of a complete device, and clearing it against the rights of others, stays with the device maker.

Public references

  1. US 3,870,405 — Helmet sight visors — 1975 patent: visor with a partially reflective inner surface; the ghost image comes from the outer surface
  2. US 6,210,858 — Anti-reflection film and display device using the same — 1997 filing: wet-coated anti-reflection film with hard coat, high-index layer and a low-index layer (n 1.20–1.55) that owes its index to micro voids

Schematic, not to scale. Layer order, indices and thicknesses are typical values from the public references; real devices differ by maker and generation. Kriya values as published on kriya-materials.com. Kriya formulates every coating for the customer's substrate, process and specification.