How long before this two-pack formulation gels?
Arrhenius 동역학을 사용하여 데이터시트 기준 온도의 가용시간을 현재 작업장 온도에서의 현실적인 작업 윈도우로 변환합니다.
How it works
A two-pack resin and hardener start to react as soon as they are mixed; the mixture's viscosity rises until the formulation can no longer be applied. The usable time, or pot life, depends on the mixing ratio, the ambient temperature and the catalyst level. It is shorter in a warm room than in a cool one.
Worked example
Arrhenius E_a 60 kJ/mol — doubling every 10 K
Arrhenius extrapolation of pot life from a reference temperature.
Validation method, references and test-case results: /validation#pot-life