Tolérance Monte Carlo
What is the yield of this stack under production variation?
Simulez les variations d'épaisseur et d'indice de réfraction par couche sur des milliers d'échantillons pour observer le comportement de votre empilement dans des conditions de production réalistes.
How it works
Manufacturing tolerance analysis samples the stack's forward model many times with layer thickness and index perturbed by their process standard deviations. The resulting distribution of the specified metric (band-averaged reflectance, colour shift, et cetera) gives the percentile bands and the yield at a given acceptance limit. The sensitivity of the yield to each parameter follows from the partial derivatives of the metric at the nominal design.
Worked example
Kriya 4-layer broadband, ±3 nm / ±0.01 n, 500 runs
Monte Carlo over thickness + n tolerances; σ(R) and yield-at-spec.
Validation method, references and test-case results: /validation#tolerance-mc