Diffusion de Mie
How do nanoparticles of this size scatter visible light?
Extinction par nanoparticules. Calcul des facteurs d'efficacité de diffusion, d'absorption et d'extinction pour une Dispersion de nanoparticules via la solution exacte de Mie (1908) aux équations de Maxwell. Transmittance d'une couche chargée par Beer-Lambert. Pour les dispersions Kriya TiO₂, ZrO₂, SiO₂, Al₂O₃ dans solvant, liant polymère ou Kriya LRI/HRI.
How it works
Mie theory gives the exact scattering and absorption cross sections of a homogeneous sphere illuminated by a plane wave, as functions of the size parameter and the complex refractive indices of sphere and host. In the small-size limit it reduces to Rayleigh scattering; around the size parameter of unity, resonances in the scattering phase function dominate.
Worked example
x = 10, m = 1.5 + 0i (Wiscombe MIEV0)
Inputs: nParticleRe = 1.5, nParticleIm = 0, nHost = 1, diameterNm = 1.751e+3, wavelengthNm = 550
Result: 2.882
Reference: Wiscombe 1980, Appl. Opt. 19, 1505; BHMIE Appendix A
Computed by this tool's kernel at build (commit dae6663).
Validation method, references and test-case results: /validation#mie-scattering