Ghost Lab

What does the eye actually see reflected off a coated surface?

Visualisez ce que l'œil perçoit. Affichez le reflet fantôme d'une scène éclairée sur une surface revêtue, sous n'importe quel angle. La luminosité et la couleur proviennent du même noyau Transfer-matrix method que le TMM Simulator.

How it works

A coated surface reflects a fraction of every wavelength in the ambient scene, weighted by the coating's spectral and angular response. Rendering that physical reflection requires combining a scene radiance distribution with the surface reflectance spectrum at each pixel and applying a camera tone curve. The transfer-matrix method supplies the reflectance input for isotropic multilayer stacks.

Worked example

Bare glass vs single-layer n 1.22 vs 4-layer, D65, 30°

Shows the ghost ladder — 4.3 % → 0.01 % → 0.3 % photopic R.

Validation method, references and test-case results: /validation#ghost-lab

Request accessOpen the interactive tool