Calculateur de couverture & coût de revêtement
What does it cost per m² to coat this substrate?
Convertit une cible d'épaisseur de film sec en consommation humide, couverture en kg et coût en €/m². Avec la géométrie de rouleau, dimensionne la demande mensuelle et la commande minimale.
How it works
The unit-area cost of a coated substrate combines the mass of coating delivered per square metre, the price of the coating formulation and the process yield. Loss factors enter through overspray, line waste and reject rate. The result is expressed per square metre of accepted good product.
Worked example
Enter solids, price and densities from your Kriya CoA, quotation and product request
Mass balance per m² and per month from your product values and the applicator settings.
Validation method, references and test-case results: /validation#coating-cost