Toutes les études de cas
Composants optiques

Le revêtement HRI thermique atteint RI > 1,8 et 8H de dureté crayon sur verre spécial

Un fabricant de verre spécial

Indicateurs clés

8HDureté crayon à RI 1,85
0.49%Haze le plus bas atteint
100%Adhérence (ASTM D3359)
130°CTempérature de durcissement minimale

01

Le défi

The glass manufacturer needed a high refractive index coating on display glass (0.7 mm) that could achieve RI 1.85 with maximum hardness. Existing HRI coatings from other suppliers could not reach 8H pencil hardness at these RI levels, and lower cure temperatures were desired to reduce energy costs.

02

Notre approche

Kriya developed three thermal-curable HRI formulation variants (V1, V2, V3), testing cure temperatures from 130°C to 200°C. Formulation optimisation focused on reducing haze through organic compound reduction (V2, V3) while maintaining RI and hardness targets. Low-outgassing variants were developed in response to customer requirements.

03

Le résultat

V1 achieved RI 1.85 and 8H pencil hardness across all cure temperatures (130–200°C). V2 delivered the lowest haze: 0.49% at 200°C cure. All variants achieved 100% adhesion (ASTM D3359). Higher cure temperatures reduced haze significantly, with the majority of improvement occurring at 160°C.

Pourquoi Kriya

Kriya’s sol-gel chemistry uniquely enables 8H pencil hardness at RI 1.85 via thermal cure alone, with tuneable cure temperatures and low-outgassing options that competitors cannot match.

Indicateurs clés

8HDureté crayon à RI 1,85
0.49%Haze le plus bas atteint
100%Adhérence (ASTM D3359)
130°CTempérature de durcissement minimale

Produits utilisés

Application associée

Optical Components →

Discuter d’une application similaire

Notre équipe technique peut vous aider à évaluer si cette approche s’applique à vos exigences spécifiques.

Démarrer une conversation