Toutes les études de cas
Solaire et énergie

Gain de transmission de 3,9 % sur verre de couverture PV avec LRI thermodurcissable

Un intégrateur de modules solaires de premier plan

Indicateurs clés

+3.9%Gain de transmission
93.8%Transmission après revêtement
630°CTrempe réussie
0.34%Haze

01

Le défi

The solar integrator needed an anti-reflective coating for photovoltaic cover glass that could increase module efficiency through higher light transmission. The coating had to survive outdoor weathering (IEC 61215) and be compatible with tempered glass processing.

02

Notre approche

Kriya applied thermal-curable LRI coating (RI 1.37) directly to the glass substrate. The coating was tested for transmission gain, haze, and tempering survival. Accelerated weathering was validated per IEC 61215 standards.

03

Le résultat

The LRI coating delivered 3.9% transmission gain (from 89.9% to 93.8% C-illuminant) with 0.34% haze. The coating survived tempering at 630°C and passed accelerated weathering validation. Direct glass coating eliminates the need for laminated AR films.

Pourquoi Kriya

Kriya’s thermal-curable LRI uniquely survives glass tempering, enabling direct application in the solar module production line without additional lamination steps.

Indicateurs clés

+3.9%Gain de transmission
93.8%Transmission après revêtement
630°CTrempe réussie
0.34%Haze

Produits utilisés

Application associée

Solar & Energy →

Discuter d’une application similaire

Notre équipe technique peut vous aider à évaluer si cette approche s’applique à vos exigences spécifiques.