Le revêtement LRI résiste à la trempe à 630 °C et offre un gain de guidage lumineux de 2,5 à 4,5×

Un leader européen du verre

Indicateurs clés

4.5×Amélioration de la luminance
+3.9%Gain de transmission
630°CTrempe réussie
0.34%Haze (illuminant C)

01

Le défi

The glass manufacturer needed an LRI coating at RI 1.37 that could survive furnace tempering (250 seconds at 630°C with rapid cooling) for use in architectural and automotive light-guiding glass. No existing LRI coating on the market was known to withstand this thermal process.

02

Notre approche

Kriya developed both UV-curable and thermal-curable LRI variants at RI 1.37. Testing included direct glass coating with low-E film, PET substrate variants, and tempering survival validation. The thermal-curable variant (095-105-C high-temperature variant) was optimised for the customer’s high-temperature process.

03

Le résultat

The thermal-curable LRI achieved 93.8% transmission (3.9% gain over uncoated substrate) with 0.34% haze. The coating survived full furnace tempering at 630°C with no visible deterioration. Light-guiding tests confirmed 2.5–4.5× luminance improvement versus uncoated glass, comparable to LRI-on-PET performance.

Pourquoi Kriya

Kriya is the only supplier offering PFAS-free overcoatable LRI that survives glass tempering temperatures, enabling direct coating of architectural and automotive glass without lamination.

Indicateurs clés

4.5×Amélioration de la luminance
+3.9%Gain de transmission
630°CTrempe réussie
0.34%Haze (illuminant C)

Produits utilisés

Application associée

Architectural Glass →

Discuter d’une application similaire

Notre équipe technique peut vous aider à évaluer si cette approche s’applique à vos exigences spécifiques.

Démarrer une conversation