Toutes les études de cas
Écrans — Pliables

Couche dure monocouche passant 200 000 cycles de pliage avec antisalissure sans PFAS

Un grand Tier-1 d'écrans coréen

Indicateurs clés

200kCycles de pliage réussis
3HPencil hardness
2,000xCycles laine d'acier réussis
>95°WCA après abrasion

01

Le défi

The OEM required a multi-functional coating for foldable displays that combined hard coating, antistatic, and antifouling properties in a single layer. The coating had to survive 200,000 fold cycles at 1.5R radius without cracking or loss of surface properties, and had to be PFAS-free to meet upcoming regulatory requirements.

02

Notre approche

Kriya formulated a UV-curable multi-functional coating (35 wt% solids) on 75 µm PET, combining hard coating, antistatic (10⁹ Ω/sq), and antifouling (WCA 110°) in a single layer. The coating was validated through exhaustive QC including 2,000-cycle steel wool abrasion, ballpoint pen drop tests, and permanent marker wipe-off testing.

03

Le résultat

The coating passed all qualification criteria: pencil hardness 3H, surface resistivity 8.0×10⁹ Ω/sq, WCA retained above 95° after 2,000 steel wool cycles at 1 kg/cm², and permanent marker wipe-off confirmed. The coating passes 200,000 fold cycles at 1.5R, compatible with R2R processing for volume production.

Pourquoi Kriya

Kriya delivered three functions in one PFAS-free layer, eliminating separate coating steps and reducing both processing cost and regulatory risk for the OEM’s foldable product line.

Indicateurs clés

200kCycles de pliage réussis
3HPencil hardness
2,000xCycles laine d'acier réussis
>95°WCA après abrasion

Produits utilisés

Application associée

Displays — Foldable →

Discuter d’une application similaire

Notre équipe technique peut vous aider à évaluer si cette approche s’applique à vos exigences spécifiques.

Démarrer une conversation