Réflectance résiduelle inférieure à 0,15 % obtenue sur empilement AR multicouche

Un fabricant de films optiques Tier-1 de premier plan

Indicateurs clés

<0.15%Réflectance résiduelle
+3.3%Gain de transmission (PET)
100%Adhérence sur tous les substrats
4Substrats validés

01

Le défi

The consumer-electronics company required a broadband anti-reflective coating stack achieving residual reflectance below 0.15% across the visible spectrum. The solution had to be PFAS-free and compatible with their existing substrate portfolio (PET, PC, PMMA, TAC).

02

Notre approche

Kriya designed a multi-layer AR stack utilising the full RI platform from 1.16 to 1.95. The stack was optimised through optical modelling and validated on four substrates, measuring transmission gain, haze, reflection, pencil hardness, and adhesion per ISO and ASTM standards.

03

Le résultat

Broadband residual reflectance below 0.15% was achieved on the multi-layer stack. Transmission gains ranged from 2.2% (PMMA) to 3.3% (PET), with 100% adhesion on all substrates. Pencil hardness varied by substrate from HB (PC) to 4H (PMMA). All formulations were PFAS-free.

Pourquoi Kriya

Kriya offers the widest PFAS-free RI range (1.16–2.00) from a single supplier, enabling complete multi-layer AR stacks without sourcing from multiple vendors.

Indicateurs clés

<0.15%Réflectance résiduelle
+3.3%Gain de transmission (PET)
100%Adhérence sur tous les substrats
4Substrats validés

Produits utilisés

Application associée

Displays →

Discuter d’une application similaire

Notre équipe technique peut vous aider à évaluer si cette approche s’applique à vos exigences spécifiques.

Démarrer une conversation