Toutes les études de cas
Thermique automobile

L'ATO dans le PVB passe le test de vieillissement accéléré de 2 000 heures

Un fabricant d'intercalaire PVB Tier-1

Indicateurs clés

2,000 hrVieillissement accéléré réussi
<0.3%Haze maintenu
PassBlocage NIR maintenu
0Dégradation significative

01

Le défi

Before committing to production integration, the Tier-1 PVB interlayer manufacturer required long-term durability validation of ATO nanoparticles in PVB under accelerated weathering conditions. Automotive glazing must maintain optical and thermal performance for the lifetime of the vehicle.

02

Notre approche

Kriya ATO in PVB samples were subjected to 2,000-hour accelerated weathering per automotive industry standards. Optical properties (transmission, haze, SHGC) and mechanical integrity were measured at intervals throughout the test programme.

03

Le résultat

All samples passed the full 2,000-hour accelerated weathering protocol with no significant degradation of optical or thermal properties. Haze remained below 0.3%, and NIR blocking performance was maintained. The results validated ATO-PVB as production-ready for automotive glazing.

Pourquoi Kriya

Kriya’s bottom-up synthesised ATO nanoparticles are inherently more stable than ball-milled alternatives because the controlled synthesis produces uniform particle size with consistent surface chemistry.

Indicateurs clés

2,000 hrVieillissement accéléré réussi
<0.3%Haze maintenu
PassBlocage NIR maintenu
0Dégradation significative

Produits utilisés

Application associée

Automotive Thermal →

Discuter d’une application similaire

Notre équipe technique peut vous aider à évaluer si cette approche s’applique à vos exigences spécifiques.

Démarrer une conversation