Toutes les études de cas
Thermique automobile

La dispersion ATO atteint 0,2–0,3 % de haze dans le PVB, validée par un partenaire Tier-1

Un fabricant d'intercalaire PVB Tier-1

Indicateurs clés

<0.3%Haze (qualité automobile)
5×Plus efficace vs concurrent à SHGC égal
~60%Coût vs ITO
75%Transmission lumière visible

01

Le défi

The Tier-1 PVB interlayer partner needed an ATO dispersion for solar heat control interlayer film that could achieve automotive-grade haze (<0.5%) when laminated with green glass. Previous ATO suppliers using top-down ball-milling produced dispersions with haze exceeding 1.7%, far above automotive requirements.

02

Notre approche

Kriya provided four ATO dispersion variants at 8.3 wt% concentration for evaluation. The partner laminated samples with 2.0 mm green glass and measured optical properties including visible light transmission, total solar transmittance, and haze according to their internal automotive qualification protocol.

03

Le résultat

The optimised variant achieved 0.2% haze at 0.10 wt% and 0.3% haze at 0.20 wt% in PVB—the only samples passing the partner’s automotive haze threshold. Visible light transmission ranged from 71–75%, and total solar transmittance from 58–61%. The partner concluded the technology had "great potential."

Pourquoi Kriya

Kriya’s proprietary bottom-up ATO synthesis produces nanoparticles with fundamentally lower scattering than ball-milled alternatives, achieving 5× better effectiveness at equal SHGC versus the leading competitor.

Indicateurs clés

<0.3%Haze (qualité automobile)
5×Plus efficace vs concurrent à SHGC égal
~60%Coût vs ITO
75%Transmission lumière visible

Produits utilisés

Application associée

Automotive Thermal →

Discuter d’une application similaire

Notre équipe technique peut vous aider à évaluer si cette approche s’applique à vos exigences spécifiques.

Démarrer une conversation