Automotive
Panoramic glass roof
Edge-lit illumination and solar heat control in one laminate
An illuminated roof uses one glass ply as a light guide, fed by LEDs at its edge and lit up by printed or laser-etched extraction patterns. PVB (n 1.48) is almost index-matched to glass (n 1.52), so in a laminate the light leaks into the interlayer within a few bounces. A thin low-index layer restores total internal reflection — and the same PVB can carry ATO to absorb solar heat.
Kriya coating position — published on kriya-materials.comKriya chemistry applies — application fit from public literatureOther device layers — not supplied by Kriya
All layers (6)
- Outer glass Tinted or privacy glass · n 1.52
- PVB interlayer with ATO n 1.48 · near-infrared absorberK1
- Low-index cladding n ≈ 1.20 · ≈ 1 µmK2
- Inner glass = light guide Low-iron glass · LEDs at the edge
- Light-extraction pattern Printed or laser-etched
- Low-E coating (optional) Not Kriya
Public references
- US 6,742,921 — Light pipe, plate light source unit and reflection type liquid-crystal display device — 2000 priority: a layer bonded to a light guide through a lower-index layer, so that guided light is totally reflected at the interface
- EP 1 447 433 — Coating material composition and article having coating film formed therewith — 2001 filing: low-index coating from fine hollow particles in a binder
More on kriya-materials.com
- kriya-materials.com/applications/automotive-thermal
- kriya-materials.com/technology/calculation-model-887
Kriya tools used on this page
Schematic, not to scale. Layer order, indices and thicknesses are typical values from the public references; real devices differ by maker and generation. Kriya values as published on kriya-materials.com. Kriya formulates every coating for the customer's substrate, process and specification.