适用期(Pot Life)定时器
How long before this two-pack formulation gels?
使用 Arrhenius 动力学,将技术规格书在参考温度下的适用期换算为当前车间温度下的实际工作窗口。
How it works
A two-pack resin and hardener start to react as soon as they are mixed; the mixture's viscosity rises until the formulation can no longer be applied. The usable time, or pot life, depends on the mixing ratio, the ambient temperature and the catalyst level. It is shorter in a warm room than in a cool one.
Worked example
Arrhenius E_a 60 kJ/mol — doubling every 10 K
Arrhenius extrapolation of pot life from a reference temperature.
Validation method, references and test-case results: /validation#pot-life