质量与制造
从纳米粒子合成到分散液配方再到最终涂层产品—整个价值链均在同一屋檐下控制。ISO 9001:2015认证。
>100k kg/yr
Dispersion capacity
1M kg/yr
Coating capacity designed
0.8 μm
Batch filtration
最多10 CTQ
每批次质量参数
最长6个月
除非另有约定(未开封)
简化制造流程
垂直整合,完全控制
从原料纳米粒子合成到最终包装产品的每一步均在内部控制。按照ISO工作程序在每个阶段进行质量检验。
Nanoparticle Synthesis
Synthesis of SiO₂, TiO₂, SnO₂, and ATO nanoparticles. Controlled particle size and narrow distribution.
Dispersion Formulation
Nanoparticles dispersed in solvent or monomer matrices at precise loading levels. Stability engineering and sub-micron filtration to ensure optical clarity.
Quality Testing
Each batch tested against up to 10 CTQ parameters before release. Samples retained for 24 months. Certificate of Analysis issued per batch.
Packaging & Dispatch
Packaging and dispatch. Worldwide shipping available.
质量保证
最多10个CTQ参数
每个生产批次在出厂前最多测试10个CTQ参数。结果记录在批次分析证书(CoA)中。
| # | Parameter | Method | Typical Tolerance | Unit |
|---|---|---|---|---|
| 1 | Refractive Index (RI) | Abbe refractometer @ 589 nm | ±0.005 of target | nD |
| 2 | Solids Content | Gravimetric (105°C, 2h) | ±1.0% of target | wt% |
| 3 | Viscosity | Brookfield DV-II+ @ 25°C | ±15% of target | mPa·s |
| 4 | Haze | BYK haze-gard plus | < 0.5% (product dependent) | % |
| 5 | Transmittance | UV-Vis spectrophotometer | > 92% @ 550 nm | %T |
| 6 | Pencil Hardness | ASTM D3363 | ≥ target grade | H scale |
| 7 | Adhesion | Cross-cut tape test (ASTM D3359) | 5B / 4B minimum | Rating |
| 8 | Surface Resistivity | Four-point probe / Hiresta | Within spec range | Ω/sq |
| 9 | Water Contact Angle | Sessile drop goniometer | Per product spec | ° |
| 10 | Shelf Life Stability | Accelerated aging (50°C, 4 weeks) | All params within spec | Pass/Fail |
生产能力
规模化能力
Kriya从研发台经过中试到生产的连续规模化路径,每个化学体系的规模化系数均已记录验证。
需要认证用的质量文件?
CoA、SDS、REACH声明和应用特定测试数据可应要求提供。