波匯出瞳擴充套件模擬器
How large is the waveguide's exit pupil for a given eyebox?
透過平面波導的二維光線追跡:視覺化入耦合、TIR 反射、出瞳複製與出耦合。實時觀察芯層折射率對眼盒尺寸的影響。
How it works
The eyebox of a waveguide display is the volume within which the eye can see the full projected image. It is set by the lateral extent and local efficiency of the out-coupling grating together with the geometry of the in-coupling and propagation stages. The visible pupil for any eye position is the intersection of these two surfaces with the eye's entrance pupil.
Worked example
n 1.80 core, 0.5 mm plate, 15 mm out-coupler, Λ 385 nm
In-coupler grating, TIR propagation, exit-pupil replication.
Validation method, references and test-case results: /validation#waveguide-pupil