VOC 排放計算器
How much volatile organic content does this formulation release?
估算年度 VOC 排放並與 EU IED 閾值進行對比。
How it works
Volatile organic content of a coating formulation is the mass fraction of solvent that evaporates during cure. It is computed from the solvent mass balance of the as-applied wet formulation. Regulatory limits are stated in grams of VOC per litre of coating ready for application.
Worked example
50 % solids waterborne at 1.05 g/mL, 5 % exempt → 450 g/L VOC
EU VOC Directive 2004/42/EC calculation from solids, density and exempt fraction.
Validation method, references and test-case results: /validation#voc-calculator