What is the yield of this stack under production variation?

對數千個樣本模擬各層厚度與折射率的變異,以了解您的膜堆設計在實際生產容差下的表現。

How it works

Manufacturing tolerance analysis samples the stack's forward model many times with layer thickness and index perturbed by their process standard deviations. The resulting distribution of the specified metric (band-averaged reflectance, colour shift, et cetera) gives the percentile bands and the yield at a given acceptance limit. The sensitivity of the yield to each parameter follows from the partial derivatives of the metric at the nominal design.

Worked example

Kriya 4-layer broadband, ±3 nm / ±0.01 n, 500 runs

Monte Carlo over thickness + n tolerances; σ(R) and yield-at-spec.

Validation method, references and test-case results: /validation#tolerance-mc