How do I extract refractive index and thickness from a transmission spectrum?

從鍍膜薄膜穿透光譜及裸基板參考光譜中提取折射率 n(λ)、消光係數 k(λ) 與物理厚度 d,包含本司針對多孔二氧化矽 LRI 鍍膜所推導之封閉式低折射率(n < s)分支。

How it works

The Swanepoel envelope method fits two smooth curves to the maxima and minima of a transmission spectrum through a thin film on a transparent substrate. The ratio and separation of the envelopes give the refractive index and the thickness; the absorption coefficient follows from the envelope average. The result depends only on the spectrum and the substrate index.

Worked example

a-Si:H envelope from Swanepoel 1983 Table 1

Transmission envelope → thickness, n(λ) via Swanepoel 1983.

Validation method, references and test-case results: /validation#swanepoel