What does a customer's reference coating appear to contain?

從測量的T(λ)和/或R(λ)識別未知堆疊。在使用者定義的材料調色盤上進行差分進化;前3名候選堆疊。

How it works

A reverse-engineering workflow combines non-destructive optical measurements (reflectance, transmittance, colour) with destructive chemical measurements (XPS, SIMS, FTIR) to constrain the likely stack architecture and materials of an unknown coating. The result is a hypothesis, not a proof — a candidate stack whose forward model matches the measurements.

Worked example

Planted 4-layer AR stack

Fit against a known planted stack; top-3 candidates ranked by residual MSE.

Validation method, references and test-case results: /validation#reverse-engineering

Request accessOpen the interactive tool