Mie 散射
How do nanoparticles of this size scatter visible light?
奈米粒子消光。利用 Mie 1908 年對 Maxwell 方程式的精確解,計算奈米粒子分散體的散射、吸收及消光效率因子。透過 Beer-Lambert 計算填充層的 Transmittance。適用於溶劑、聚合物黏結劑或 Kriya LRI/HRI 中的 Kriya TiO₂、ZrO₂、SiO₂、Al₂O₃ 分散體。
How it works
Mie theory gives the exact scattering and absorption cross sections of a homogeneous sphere illuminated by a plane wave, as functions of the size parameter and the complex refractive indices of sphere and host. In the small-size limit it reduces to Rayleigh scattering; around the size parameter of unity, resonances in the scattering phase function dominate.
Worked example
x = 10, m = 1.5 + 0i (Wiscombe MIEV0)
Inputs: nParticleRe = 1.5, nParticleIm = 0, nHost = 1, diameterNm = 1.751e+3, wavelengthNm = 550
Result: 2.882
Reference: Wiscombe 1980, Appl. Opt. 19, 1505; BHMIE Appendix A
Computed by this tool's kernel at build (commit dae6663).
Validation method, references and test-case results: /validation#mie-scattering