How does nanoparticle loading change the refractive index of a coating?
從第一原理出發設計低折射率塗層:中空奈米顆粒的幾何引數(殼厚、直徑、堆積密度)透過兩級有效介質理論決定有效折射率。
How it works
Adding nanoparticles to a polymer host shifts the effective refractive index of the mixture toward the index of the particles. Effective-medium theories (Maxwell-Garnett at low fractions, Bruggeman at higher) relate the loading, host and particle indices to the mixture index. Process-side constraints on viscosity and film continuity bound the practical loading range.
Worked example
Hollow silica 60 nm, shell 8 nm, 55 vol % in binder 1.49
Hollow-silica particles in a binder; Maxwell-Garnett for both the particle and film mixing steps.