CTE 不匹配翹曲

How large are the thermal-cycling stresses between these two layers?

預測熱膨脹不匹配應力、基板曲率及邊緣垂度(鍍膜與基板同步固化冷卻時)。標示微影/取放/搬運作業的閾值。

How it works

A thin coating bonded to a substrate experiences in-plane strain when the two materials have different coefficients of thermal expansion and the stack is heated or cooled. For a thin film on a thick substrate, Stoney's approximation relates the induced stress to the differential strain, the film's biaxial modulus and the temperature change. Plasticity, cracking and delamination follow once the stress exceeds the film's fracture or adhesion strength.

Worked example

PC 1 mm substrate, ΔT 60 K

CTE mismatch × ΔT → biaxial film stress and substrate warpage via Stoney.

Validation method, references and test-case results: /validation#cte-mismatch

Request accessOpen the interactive tool