寬頻 AR 疊層最佳化器

Which layer thicknesses minimise reflectance across a target band?

針對目標波長範圍,基於 Kriya 材料庫找出使平均反射率最小的各層厚度。

How it works

Multilayer anti-reflection design minimises the band-averaged reflectance of a stack by varying the thickness of each layer. A forward optical model such as the transfer-matrix method evaluates the reflectance for any trial thickness vector; a global optimiser such as differential evolution searches that space for a minimum subject to layer-count and index constraints.

Worked example

Target R < 0.5 % 420–680 nm on PMMA

4-layer stack from the Kriya LRI 1.35 / HRI 1.65 library.

Validation method, references and test-case results: /validation#ar-optimizer

Request accessOpen the interactive tool